Strong Sintered Disc SmCo Magnet

  • Price:

    Negotiable

  • minimum:

  • Total supply:

  • Delivery term:

    The date of payment from buyers deliver within days

  • seat:

    Zhejiang

  • Validity to:

    Long-term effective

  • Last update:

    2017-12-01 11:09

  • Browse the number:

    148

Send an inquiries

Company Profile

Ningbo Sine Magnetic Co., Ltd.

By certification [File Integrity]

Contact:Ms. Gabriel(Mr.)  

Email:

Telephone:

Area:Zhejiang

Address:Zhejiang

Website: http://nbsine.gdzhongbang.com/

Product details
Strong sintered disc SmCo magnet

Brief introduction about SmCo magnets:

Samarium Cobalt rare-earth (SmCo) magnets are manufactured by using powder metallurgy techniques which include stringent process controls and complicated heat treatment cycles. The composition of this alloy is approximately 35% Samarium, 60% cobalt with the balance being Fe& Cu.

1. Superior resistance to high temperature.

2. Excellent resistance to corrosion, no coating is needed for surface protecting.

3. High working temperature.

4. SmCo is suitable for machines with high magnetic requirements and good for strict working environment requirements.

5. Common uses in different fields.
All sorts of SmCo are used in the Electronic Magnetron, Magnetic Transmission, Magnetic Treatment, Magnistor, etc
Technical data of SmCo Magnet
Material Grade Energy Product(BH)max Residual Induction Br(min-max) Coercive Force Hcb(min-max) Intrinsic Coercive Force Hcj(min-max) Density D Rev. Tenp Coeff α(Br) Curie Temp TC Max Working Temp Tw
KJ/m 3 MGsOe T KGs KA/m KOe KA/m KOe g/cm 3 %/ºC ºC ºC
SmCo5 XG16 120~143 15~18 0.77-0.86 7.7-8.6 613-716 7.7-9.0 ≥1194 ≥15.0 8.3 -0.04 ≥740 250
XG16H 120~143 15~18 0.77-0.86 7.7-8.6 613-716 7.7-9.0 ≥1592 ≥20.0
XG18 135~159 17~20 0.81~0.92 8.1~9.2 637~756 8.0~9.5 ≥1194 ≥15.0
XG18H 135~159 17~20 0.81~0.92 8.1~9.2 637~756 8.0~9.5 ≥1592 ≥20.0
XG20 151~175 19~22 0.85~0.95 8.5~9.5 637~756 8.0~9.5 ≥1194 ≥15.0
XG20H 151~175 19~22 0.85~0.95 8.5~9.5 637~756 8.0~9.5 ≥1592 ≥20.0
XG22 167~191 21~24 0.89~1.0 8.9~10.0 661~772 8.3~9.7 ≥1194 ≥15.0
XG22H 167~191 21~24 0.89~1.0 8.9~10.0 661~772 8.3~9.7 ≥1592 ≥20.0
Sm2Co17 XGS24M 175~199 22~25 0.92~1.04 9.2~10.4 318~788 4.0~9.9 398~1194 5.0~15.0 8.4 -0.03 ≥850 350
XGS24 175~199 22~25 0.92~1.04 9.2~10.4 661~796 8.3~10.0 1194~1990 15.0~25.0
XGS24H 175~199 22~25 0.92~1.04 9.2~10.4 661~804 8.3~10.1 > 1990 > 25.0
XGS26M 191~215 24~27 1.0~1.06 10.0~10.6 318~796 4.0~10.0 398~1194 5.0~15.0
XGS26 191~215 24~27 1.0~1.06 10.0~10.6 677~820 8.5~10.3 1194~1990 15.0~25.0
XGS26H 191~215 24~27 1.0~1.06 10.0~10.6 677~820 8.5~10.3 > 1990 > 25.0
XGS28M 207~231 26~29 1.04~1.10 10.4~11.0 318~804 4.0~10.1 398~1194 5.0~15.0
XGS28 207~231 26~29 1.04~1.10 10.4~11.0 677~820 8.5~10.3 1194~1990 15.0~25.0
XGS28H 207~231 26~29 1.04~1.10 10.4~11.0 677~820 8.5~10.3 > 1990 > 25.0
XGS30M 223~247 28~31 1.07~1.12 10.7~11.2 318~804 4.0~10.1 398~1194 5.0~15.0
XGS30 223~247 28~31 1.07~1.12 10.7~11.2 700~828 8.8~10.4 1194~1990 15.0~25.0
XGS30H 223~247 28~31 1.07~1.12 10.7~11.2 700~828 8.8~10.4 > 1990 > 25.0
XGS32M 231~255 29~32 1.09~1.15 10.9~11.5 318~804 4.0~10.1 398~955 5.0~12.0
XGS32 231~255 29~32 1.09~1.15 10.9~11.5 716~836 9.0~10.5 > 955 > 12.0
Low Temp Coeff Sm2Co17 XGS22LT 159~183 20~23 0.90~0.99 9.0~9.9 677~756 8.5~9.5 ≥1194 ≥15.0 8.4 -0.015 ≥850 350
XGS24LT 175~199 22~25 0.92~1.02 9.2~10.2 677~756 8.5~9.5 ≥1194 ≥15.0